Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Chemicals Soda Solvay® Dense Soda Ash (European Grade)

Category Fluid
Manufacturer Solvay Chemicals
Trade Name Soda Solvay®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Chemicals Soda Solvay® Dense Soda Ash (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass industry – Raw Material for melting; Chemical industry – Production of sodium derivatives; Detergents- Alkaline support; Metallurgical processes – Desulfurization of pig iron – Raw material for melting and Flue gas treatment – Removal of acidic components CAS Number: 497-19-8/EINECS: 207-838-8Information provided by Solvay
Physical Properties Metric English Comments
Density 1.02 - 1.13 g/cc
0.0368 - 0.0408 lb/in³
Free flowing, Typical
0.950 - 1.20 g/cc
0.0343 - 0.0434 lb/in³
Free flowing, Specification
2.533 g/cc
0.09151 lb/in³
Solubility in Water 21.4 %
21.4 %
pH 11.26
11.26
1% in water
Molecular Weight 106 g/mol
106 g/mol
Thermal Properties Metric English Comments
Melting Point 851 °C
1560 °F
Descriptive Properties Value Comments
Composition <0.04%
Na2SO4, Specification
<0.15%
NaCl, Specification
<150 ppm
MgO, Specification
<21 ppm
Fe2O3, Specification
<280 ppm
CaO, Specification
>99%
Na2CO3, Specification
0.0013
NaCl, Typical
0.01-0.02%
Na2SO4, Typical
0.579
Na2O, Specification
0.583
Na2O, Typical
0.996
Na2CO3, Typical
2-10 ppm
Fe2O3, Typical
32-100 ppm
CaO, Typical
40-118 ppm
MgO, Typical
Granulometry <1%
&gt;2 mm, Specification
<10%
&lt;0.125 mm, Specification
<15%
&gt;1 mm, Specification
0.2-1.0%
&lt;0.063 mm, Specification
0.4-7.0%
&gt;1 mm, Typical
0-0.3%
&gt;2 mm, Typical
1.6-3%
&gt;0.125 mm, Typical
12-40%
&gt;0.5 mm, Typical
Loss on drying <0.5%
Specification
0.12-0.2%