Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 851 °C | 1560 °F | |
Solvay Chemicals Soda Solvay® Dense Soda Ash (European Grade) Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
Melting Point | 851 °C | 1560 °F | |
Solvay Chemicals Soda Solvay® Light Soda Ash (European Grade) Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
Melting Point | 851 °C | 1560 °F | |
Solvay Chemicals Soda Solvay® Dense Soda Ash Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |