Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.533 g/cc | 0.09151 lb/in³ | |
Solvay Chemicals Soda Solvay® Dense Soda Ash (European Grade) Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
Density | 2.533 g/cc | 0.09151 lb/in³ | |
Solvay Chemicals Soda Solvay® Light Soda Ash (European Grade) Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
Density | 2.533 g/cc | 0.09151 lb/in³ | |
Solvay Chemicals Soda Solvay® Dense Soda Ash Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
Density | 2.533 g/cc | 0.09151 lb/in³ | |
American Elements Silicon Oxide Nanopowder General DescriptionSilicon Oxide (SiO2) Nanopowder, Silica Nanoparticles or nanodots are high surface area particles. Nanoscale Silicon Oxide Nanoparticles or Silica Particles are typically 5 - 100 .. |