Polymer Property : Density = 0.09151 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.533 g/cc
0.09151 lb/in³
Solvay Chemicals Soda Solvay® Dense Soda Ash (European Grade)
Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in..
Density 2.533 g/cc
0.09151 lb/in³
Solvay Chemicals Soda Solvay® Light Soda Ash (European Grade)
Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in..
Density 2.533 g/cc
0.09151 lb/in³
Solvay Chemicals Soda Solvay® Dense Soda Ash
Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in..
Density 2.533 g/cc
0.09151 lb/in³
American Elements Silicon Oxide Nanopowder
General DescriptionSilicon Oxide (SiO2) Nanopowder, Silica Nanoparticles or nanodots are high surface area particles. Nanoscale Silicon Oxide Nanoparticles or Silica Particles are typically 5 - 100 ..