Physical Properties Metric English Comments
Melt Index of Compound 25 - 31 g/10 min

@Load 2.16 kg,
Temperature 250 °C
25 - 31 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity
Information from Shinkong Synthetic Fibers Corp.
Melt Index of Compound 25 - 31 g/10 min

@Load 2.16 kg,
Temperature 250 °C
25 - 31 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity
Information from Shinkong Synthetic Fibers Corp.