Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 65FS LB PC/ABS-Blend Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 85V PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 90VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T25020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPHC TS25020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB SCANBLEND FS8 ASUV4 PC/ASA, Antistatic, Improved Weather Resistance Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 230 °C |
25 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB SCANBLEND SS7 PC/ASA, UV-Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 250 °C |
25 g/10 min @Load 4.76 lb, Temperature 482 °F |
±5; cm³/10min; ISO 1133 |
PolyOne Bergadur™ PB40 G15 blue Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP COLORCOMP EX12304C PEI (Asia Pacific) LNP* Colorcomp* EX12304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS technol.. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF35040 D PP, Glass Fiber-Reinforced, Chemically Coupled, Detergent Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 21.6 kg, Temperature 190 °C |
25 g/10 min @Load 47.6 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Melt Index of Compound | 25 g/10 min @Load 21.6 kg, Temperature 190 °C |
25 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Huntsman IROGRAN® PS442-202 TPU-Polyester Introduction: IROGRAN PS440-202 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN PS440-202 is part of the HUNTSMAN .. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 190 °C |
25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5004 1000 Micron EVA Powder Description: ICOFLO 510-5004 is an EVA powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (inste.. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 190 °C |
25 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Meilian Chemical PE12086 WHITE MASTERBATCH WHITE PE12086 is a white low density polyethylene based masterbatch highly-concentrated with TiO2 without any addition of filler and fluorescence whitener. This product is designed for general-purpo.. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1010K PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 9011 PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). Resin is RoHS compliant. Improved processability for Fiber extrusion. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM HU1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 265 °C |
25 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Melt Index of Compound | 25 g/10 min | 25 g/10 min | |
Sibur PL-1GS Polyvinyl Chloride (PVC) For the production of boot tops and soles of autumn-spring purpose and for production of boots by molding method under pressure. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 250 °C |
25 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 280 °C |
25 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL EXNL1117 PPE+HIPS high gloss Noryl |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 280 °C |
25 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Asia Pacific) high gloss Noryl |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 190 °C |
25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Melt Index of Compound | 25 g/10 min | 25 g/10 min | ASTM D1238 |
Cheng Yu Plastic 3265 TPE Rubber |
|||
Melt Index of Compound | 25 g/10 min @Temperature 230 °C |
25 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ P48U Polyester TPE, Weather-resistant Features: Polyester TPE, Weather-resistantInformation provided by Toyobo. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM AUT200 PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperatu.. |