Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
16.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87350 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 8.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
16.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87850 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 8.83 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
16.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinblend® A724 PC/PBT, High Impact Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 8.80 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
16.5 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Compression Molded, all hinge breaks; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 8.83 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
16.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinblend® A724 PC/PBT, High Impact Information from Shinkong Synthetic Fibers Corp. |