Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 700000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
700000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 2014 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Viscosity | 700000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
700000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 1E554 Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Viscosity | 700000 cP @Temperature 160 °C |
700000 cP @Temperature 320 °F |
Melt viscosity @ 2.16 kg; ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 100 Linear Thermoplastic Polyurethane Pearlbond™ 100 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve.. |
|||
Viscosity | 700000 cP | 700000 cP | |
Momentive Performance Materials RTV577 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the stand.. |
|||
Viscosity | 700000 cP @Temperature 25.0 °C |
700000 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV577 White Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Viscosity | 700000 cP | 700000 cP | Melt Viscosity; SABIC Method |
SABIC Innovative Plastics Valox® 315 PBT Unreinforced, For extrusion/compounding only (not for injection molding). High viscosity. Melt viscosity between 7500 and 9500 poise. |
|||
Viscosity | 700000 cP | 700000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE2090-60AB Elastomer KE-2090-60 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Viscosity | 700000 cP | 700000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE2090-40AB Elastomer KE-2090-40 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Viscosity | 700000 cP | 700000 cP | A |
Shin-Etsu Silicones LIMSâ„¢ KEG2002-60A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 700000 cP | 700000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KEG2002-60A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 700000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
700000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 3860 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Viscosity | 700000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
700000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® E418 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Viscosity | 700000 cP | 700000 cP | |
Esstech X-950-0000 BisGMA Resin, C29H36O8 Bisphenol A Glycidyl Methacrylate or bis-GMA is a high viscosity resin that has been used in dental formulations for years. Our BisGMA is manufactured with low levels of BPA or bisphenol A and low c.. |
|||
Viscosity | 700000 cP @Shear Rate 300 1/s, Temperature 190 °C |
700000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys Alcryn® 2080 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Viscosity | 700000 - 1.10e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
700000 - 1.10e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
Arkema Group KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Viscosity | 700000 cP | 700000 cP | Mixed; TM R050-12 |
Resinlab® EP11HT Gray Filled Epoxy Adhesive Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |
|||
Viscosity | 700000 cP | 700000 cP | Part B, RVT, #7, 2.5 rpm; TM R050-12 |
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |
|||
Viscosity | 700000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
700000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
|
DuPont Bynel® 2169 Anhydride-Modified Ethylene Acrylate Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |
|||
Viscosity | 700000 cP @Temperature 420 °C |
700000 cP @Temperature 788 °F |
melt; ISO 11443 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |