Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | STN EN ISO 294-4 |
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Oxford Polymers C-Acetal 25GF 25% Glass Fiber Reinforced Copolymer Acetal 25% Glass Fiber Reinforced Copolymer AcetalInformation provided by Oxford Polymers. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PBT 1455 PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | STN 64 0808 |
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Lubri-Tech™ PS-000/15T-2S Polyester (PBT) - 15% PTFE Lubricated - 2% Silicone Lubricated
(discontinue Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 80.0 mm |
0.022 in/in @Thickness 3.15 in |
sheet; ASTM D4894 |
3M Dyneon™ TF 4246 PTFE 35% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Linear Mold Shrinkage | 0.022 - 0.027 cm/cm | 0.022 - 0.027 in/in | ASTM D955 |
Kolon SPESIN® KP213HIBL Impact Resistant PBT Compound resin Impact resistant, BLACKApplications: Wiper bladesInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE2090-70AB Elastomer KE-2090-70 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
SK Chemicals SKYPEL G182D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-35A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aclo Accucomp Polyacetal (POM) ACE091L High Viscosity |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPP 200-2 PP Black Polypropylene Copolymer AAROLENE® ARPP 200 Series Polypropylene Compounded ResinFeatures: A high flow polypropylene copolymer resin, pre-colored black, specifically designed for all high speed injection molding applicati.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPP 200-4 PP Black Polypropylene Copolymer, No Break AAROLENE® ARPP 200-4 Series Polypropylene Compounded ResinFeatures: A copolymer polypropylene resin, pre-colored black, featuring excellent toughness for all extrusion applications. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPP C 200-3 Polypropylene Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AVPP C 200-2 Virgin Polypropylene Melt flow index may be specified. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AVPP HOMO 200-1 Virgin Polypropylene A virgin polypropylene specifically designed for all injection molding applications. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 4.00 mm |
0.022 in/in @Thickness 0.157 in |
|
Azoty Tarnow™ TARNOFORM 300 CI4 POM Impact modified injection molding grade based on Tarnoform 300 reinforced with 20% MBS rubber yielding good cold impact strength and good strength of weld lines combined with good weatherability.Inf.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, Conditioned Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® 197-N2 Acetal A general purpose, very low viscosity, in natural.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPP H 200-1 PP Black Polypropylene Homopolymer Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinFeatures: A pre-colored, black homopolymer polypropylene resin specifically designed for all injection molding applications.High Flow |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | 0.125; ASTM D955 |
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Mitsubishi Iupital® F10-02 High Viscosity Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |