Shandong Guangyin 1212 Reinforced Nylon

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer Shandong Guangyin
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Guangyin 1212 Reinforced Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features and Applications: Wear resistance, higher strength, better tenacity, strong adhesion and better low temperature resistance. It is applicable to surface coating of wires, cables, optical cables, metal wires or ropes.Information provided by Shandong Guangyin
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
Elongation at Break 6.0 %
6.0 %
Flexural Strength 145 MPa
21000 psi
Flexural Modulus 5.50 GPa
798 ksi
Izod Impact, Notched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
Izod Impact, Unnotched (ISO) 120 kJ/m²
57.1 ft-lb/in²