Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROPRENE® ATPR 1000 70A Elastomeric Compound

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® ATPR
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® ATPR 1000 70A Elastomeric Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
"E"; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 67 - 73
67 - 73
ASTM D2240
Tensile Strength 6.89 MPa
1000 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Tensile Modulus 0.00276 GPa
0.400 ksi
ASTM D412
Tear Strength 35.1 kN/m
200 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 360
360
H-18; ASTM D1044