Material Notes:
Solder Pallet and Work Holder Sheet A Static dissipative sheet material for use in electronic assembly. Resistant to hot solder and solvents. Standard color is blue/grey. Available thicknesses from 1/8" to 1/2" and 4mm to 12mm. Sheet sizes are 36" X 72" and 48" X 60", special thicknesses and custom sheet sizes are available.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ASTM D572
Water Absorption 0.75 %
0.75 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 30
30
Tensile Strength, Ultimate 41.0 MPa
5950 psi
Flexural Strength 100 MPa
14500 psi
Compressive Strength 152 MPa
22000 psi
Izod Impact, Notched 4.30 J/cm
8.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Surface Resistance 1e+05 - 1.00e+9 ohm
1e+05 - 1.00e+9 ohm
Ohm; ASTM D257