Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samyang Trirex® SF3200GNH20 Polycarbonate, Reinforced Non Halogen for Printers

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 20% Glass Filled
Manufacturer Samyang
Trade Name Trirex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Trirex® SF3200GNH20 Polycarbonate, Reinforced Non Halogen for Printers.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.SF3200GNH20 is a reinforced, non-halogen grade for Printers.Applications: Office Machine (O/A, Printer) Internal PartsInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Water Absorption 0.12 %
0.12 %
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Melt Flow 22 g/10 min

@Load 1.20 kg,
Temperature 300 °C
22 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength 98.1 MPa
14200 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Yield Strength 108 MPa
15600 psi
ASTM D790
Flexural Modulus 7.65 GPa
1110 ksi
ASTM D790
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 31.0 µm/m-°C
17.2 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
252 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.11
3.11
ASTM D150
Dielectric Strength 31.0 kV/mm
787 kV/in
ASTM D149
Dissipation Factor 0.0090
0.0090
ASTM D150
Arc Resistance 120 sec
120 sec
ASTM D495
Copyright © lookpolymers.com All Rights Reserved