Mechanical Properties Metric English Comments
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
PolyMirae Moplen HP310R Extrusion Coating and Lamination Grade Polypropylene
Moplen HP310R is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP310R is a copolymer particularly suitable for extrusion coating and..
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
Kolon Kocetal® EC701 Modified Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
Kolon Kocetal® DP301 Modified Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
Kolon Kocetal® VT701 Modified Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Izod Impact, Notched 0.588 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUCEL N127LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
Izod Impact, Notched 0.588 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUCON CP2100-KA02 PC+CF
Description Injection Molding Grade, PC+CF, Electrostatic Dissipation, Low Surface ResistanceApplication: LCD Tray, HDD BracketCAS No. 103598-77-2 and 7440-44-0Information provided by LG Chemical
Izod Impact, Notched 0.588 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant
Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG..
Izod Impact, Notched 0.588 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage
Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
DIN 53453; ASTM D256
Kolon KOPA® KN333HB640BL Multi Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Izod Impact, Notched >= 0.588 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
>= 1.10 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOL HI5302A PP+MF15%, High Impact
Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical
Izod Impact, Notched 0.588 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical Lupox® GP1006FD PBT
Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica..
Izod Impact, Notched 0.588 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical Lupox® GP2200 PBT+GF20%
Description: Injection Molding, PBT+GF20%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
Izod Impact, Notched 0.588 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical Lupox® NH2306F PBT+GF30%
Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
Izod Impact, Notched >= 0.588 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 1.10 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY ER5151RFA PC/ABS Mineral Filler, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High strength, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 14807-96-6Information p..
Izod Impact, Notched >= 0.588 J/cm

@Thickness 6.35 mm
>= 1.10 ft-lb/in

@Thickness 0.250 in
ASTM D256
Gromax CCP PBT 1100-211X
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
Lotte Chemical Titan TITANZEX® HI2200 High density polyethylene
HI2200 is a high density polyethylene for injection molding. HI2200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a.Ap..
Izod Impact, Notched >= 0.588 J/cm

@Thickness 6.35 mm
>= 1.10 ft-lb/in

@Thickness 0.250 in
ASTM D256
Gromax PBT 1100-211S
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
DIN 53453; ASTM D256
Kolon KOPA® KN178MT40 M/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
Shinil Chemical SHINCON PSU-CNT LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
Shinil Chemical SHINNANO PA-6 Polymer Nanocomposite Air Intake Module
SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using..
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Shinkong Synthetic Fibers Shinite® T102G15 PET, 15% Glass Filled, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® XP-2165MC PPS
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samyang Trilen® 9550AC Polypropylene, General Purpose
Mechanical strength and thermal resistance are excellent.9550AC is a general purpose grade.Applications: ConnectorsInformation provided by Samyang.
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing
Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi..
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
E-Polymers SEPAZ® V220A 20% Glass Fiber Reinforced PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
E-Polymers TEKAMID® H12TW Unreinforced Low warpage PA/ABS Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB..
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Asia International Enterprise (Hong Kong) 60G3F Nylon 66, 15% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Izod Impact, Notched 0.588 J/cm

@Temperature 23.0 °C
1.10 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LG Chemical LUTENE-H ME8000 HDPE
Description: LUTENE-H ME8000 is mainly intended for injection molding of containers. It has good mechanical properties and high productivity.Applications: Silicone cartridge, containers, complicated..
Copyright © lookpolymers.com All Rights Reserved