Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Melt Flow 46 g/10 min

@Load 10.0 kg,
Temperature 220 °C
46 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Flexural Strength 83.4 MPa
12100 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.35 GPa
341 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 5.88 J/cm

@Thickness 3.17 mm
11.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C

@Thickness 6.40 mm
208 °F

@Thickness 0.252 in
ASTM D648
UL RTI, Electrical 85.0 °C
185 °F
UL RTI, Mechanical with Impact 85.0 °C
185 °F
UL RTI, Mechanical without Impact 85.0 °C
185 °F
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
V-0

@Thickness 2.00 - 3.00 mm
V-0

@Thickness 0.0787 - 0.118 in
5VB

@Thickness 2.00 - 3.00 mm
5VB

@Thickness 0.0787 - 0.118 in