Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 46 - 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
46 - 50 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers NPP 50-5052 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Melt Flow | 46 g/10 min @Load 2.16 kg, Temperature 330 °C |
46 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. |
|||
Melt Flow | 46 g/10 min @Load 2.16 kg, Temperature 330 °C |
46 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 46 g/10 min @Load 2.16 kg, Temperature 330 °C |
46 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 46 g/10 min @Load 2.16 kg, Temperature 330 °C |
46 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 46 g/10 min @Load 2.16 kg, Temperature 330 °C |
46 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East) XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 46 g/10 min @Load 2.16 kg, Temperature 330 °C |
46 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Melt Flow | 46 g/10 min @Load 2.16 kg, Temperature 330 °C |
46 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Melt Flow | 46 g/10 min @Load 5.00 kg, Temperature 190 °C |
46 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 57 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60.. |
|||
Melt Flow | 46 g/10 min @Load 2.16 kg, Temperature 330 °C |
46 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Melt Flow | 46 g/10 min @Load 2.16 kg, Temperature 320 °C |
46 g/10 min @Load 4.76 lb, Temperature 608 °F |
ASTM D1238 |
Kuraray Genestarâ„¢ G1302 Nylon, 30% Glass Filled Abrasion Resistance HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It delivers low.. |
|||
Melt Flow | 46 g/10 min @Load 10.0 kg, Temperature 220 °C |
46 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 46 g/10 min @Load 10.0 kg, Temperature 220 °C |
46 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 46 g/10 min @Load 10.0 kg, Temperature 220 °C |
46 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 46 g/10 min @Load 10.0 kg, Temperature 220 °C |
46 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 46 g/10 min @Load 5.00 kg, Temperature 200 °C |
46 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex TEKBOND® 6000-75 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 46 g/10 min @Load 2.16 kg, Temperature 330 °C |
46 g/10 min @Load 4.76 lb, Temperature 626 °F |
ISO 1133 |
Covestro Apec® 1697 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Melt Flow | 46 - 54 g/10 min @Load 2.16 kg, Temperature 230 °C |
46 - 54 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
AKG Polymers Vision PP PPC BL5005 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Melt Flow | 46 - 54 g/10 min @Load 2.16 kg, Temperature 230 °C |
46 - 54 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
AKG Polymers Vision PP PPH BL5003 Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Melt Flow | 46 g/10 min @Load 14.91 kg, Temperature 175 °C |
46 g/10 min @Load 32.87 lb, Temperature 347 °F |
ASTM D-1238 |
Axiall 1701 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |