Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 742L-13G Nylon 6/66, 13% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 10% Glass Fiber Reinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 742L-13G Nylon 6/66, 13% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
6/66 Copolymer with high surface gloss in addition to high stiffness and strength, 13% Glass Reinforced.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ASTM D638
Elongation at Break 7.5 %
7.5 %
Flexural Modulus 3.60 GPa
522 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
261 °F
ASTM D648