Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.7 MPa
9250 psi
50 mm/min; ASTM D638
Flexural Strength 94.1 MPa
13600 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.75 GPa
398 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 3.92 J/cm

@Thickness 3.17 mm
7.35 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C

@Thickness 6.40 mm
205 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in