Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.75 GPa

@Thickness 3.20 mm
398 ksi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical HI121H ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Flexural Modulus 2.75 GPa

@Thickness 3.20 mm
398 ksi

@Thickness 0.126 in
15mm/min; ASTM D790
LG Chemical LUCON CP6062EX PC/ABS+CNT
Description: Sheet Extrusion or Injection Molding, PC/ABS+CNT, Electrostatic Dissipation, Wide Processing Range, Low Surface ResistivityApplication: BLU Carrying TrayCAS No. 103598-77-2, 9003-56-9, ..
Flexural Modulus 2.75 GPa
398 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN111 General Purpose Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 2.75 GPa

@Thickness 3.20 mm
398 ksi

@Thickness 0.126 in
2.8mm/min; ASTM D790
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity
Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical
Flexural Modulus 2.75 GPa

@Thickness 3.20 mm
398 ksi

@Thickness 0.126 in
15mm/min; ASTM D790
LG Chemical LUMIPLAS LD590 Light diffusion ABS
Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical
Flexural Modulus 2.75 GPa

@Thickness 6.40 mm
398 ksi

@Thickness 0.252 in
1.3mm/min; ASTM D790
LG Chemical LUPOL GP2150 PP+GF15%
Description: Injection Molding, PP+GF15%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical
Flexural Modulus 2.75 GPa

@Thickness 6.40 mm
398 ksi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL GP3200 PP+MF20%
Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Flexural Modulus 2.75 GPa
398 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN333HRN Heat Resistant Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Flexural Modulus 2.75 GPa

@Thickness 3.20 mm
398 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch..
Flexural Modulus 2.75 GPa

@Thickness 3.20 mm
398 ksi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical PI642G ABS, General Purpose, High Modulus
Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical
Flexural Modulus 2.75 GPa
398 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN133HR Heat Resistant Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 2.75 GPa

@Thickness 6.40 mm
398 ksi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL HR2100D PP+GF17%
Description: Injection Molding, PP+GF17%, General PurposeApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 165997-17-3Information provided by LG Chemical
Flexural Modulus 2.75 GPa

@Thickness 3.20 mm
398 ksi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical XG568 MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
Flexural Modulus 2.75 GPa
398 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 2.75 GPa
398 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 2.74 GPa
398 ksi
ASTM D790
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 2.74 GPa
398 ksi
ASTM D790
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 2.74 GPa
398 ksi
ASTM D790
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 2.74 GPa
398 ksi
ASTM D790
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 2.74 GPa
398 ksi
ASTM D790
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 2.74 GPa
398 ksi
ASTM D790
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 2.75 GPa

@Thickness 6.40 mm
398 ksi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade
Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali
Flexural Modulus 2.75 GPa
398 ksi
2.8mm/min; ASTM D790
Asia International Enterprise (Hong Kong) 3010F Polybutylene terephthalate
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Flexural Modulus 2.74 GPa
398 ksi
ASTM D790
Aaron Industries AAROPRENE® AEN 6000-1 Nylon 6 Engineered Resin
Flexural Modulus 2.75 GPa

@Thickness 3.20 mm
398 ksi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 6605 Toughened Polystyrene
Characteristics Excellent melt strength High stiffness Easy tearability Processing Extrusion Applications Suitable for thin film for candy wrap and window envelope Economic production of clear th..
Flexural Modulus 2.74 GPa
398 ksi
ASTM D790
Quadrant EPP Quadrant PVC Polyvinyl Chloride, Type I, Grade 1 (ASTM Product Data Sheet)
Flexural Modulus 2.75 GPa

@Thickness 6.40 mm
398 ksi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade
Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali
Copyright © lookpolymers.com All Rights Reserved