Mechanical Properties Metric English Comments
Izod Impact, Notched 3.92 J/cm
7.35 ft-lb/in
ASTM D256
Global MB-6366 High Density Polyethylene
Description-high density for high quality, excellent creep & chemical resistanceApplications-drinking water pipe, industrial pipe, sewer pipeInformation provided by Global Polymers Corporation.
Izod Impact, Notched 3.92 J/cm
7.35 ft-lb/in
ASTM D256 A
GRECO ISOPAK 640 Polycarbonate/ABS Alloy
Flame retardant polycarbonate/ABS alloy; good impact and dimensional stabilityInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Izod Impact, Notched >= 3.92 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 7.35 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical..
Izod Impact, Notched 3.92 J/cm

@Thickness 3.17 mm
7.35 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 6.35 mm
7.35 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® SD-0190H ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 3.17 mm
7.35 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm

@Thickness 6.35 mm
7.35 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® SD-0190H ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.92 J/cm
7.35 ft-lb/in
Zylog Hipolyene® 8501 T6 B Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Izod Impact, Notched 3.92 J/cm
7.35 ft-lb/in
ASTM D256
Cheng Yu Plastic A778 Electric Resisting ABS
Izod Impact, Notched 3.92 J/cm
7.35 ft-lb/in
ASTM D256
Cheng Yu Plastic A779 Lubrication ABS