Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CPC - Vycom Corzan® CPVC Chlorinated PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer CPC - Vycom Co.
Trade Name Corzan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPC - Vycom Corzan® CPVC Chlorinated PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Corzan CPVC is a high heat, corrosion resistant chlorinated polyvinyl chloride (CPVC) sheet. Because of its excellent corrosion resistance at elevated temperatures, it is ideally suited for self-supporting constructions where high temperatures are a concern. It can be used (depending on chemistry) up to 180º F. Corzan CPVC conforms to ASTM-D-1784-95 Class 23447-B (formerly Type IV Grade 1) and is manufactured without fillers or plasticizers.FEATURES AND BENEFITS System compatibility- Corzan is available in pipe, valves, fitting and sheet to construct completely compatible systems. Machinable- Corzan can be machined, cut, routed and welded. Flammability- Corzan is self extinguishing and has a flame spread of less than 20. Physical properties- Corzan has outstanding strength through a range of temperatures. Impact- Corzan has excellent impact strength. Chemical resistance- Corzan has excellent chemical resistance to acids and alkalis.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Ultimate 50.3 MPa
7300 psi
ASTM D638
Flexural Strength 98.6 MPa
14300 psi
ASTM D790
Flexural Modulus 2.49 GPa
361 ksi
ASTM D790
Compressive Strength 69.6 MPa
10100 psi
ASTM D695
Compressive Modulus 1.35 GPa
196 ksi
ASTM D695
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 69.5 µm/m-°C

@Temperature 20.0 °C
38.6 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.140 W/m-K
0.972 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
ASTM D648
Flammability, UL94 5VB
5VB
0.062 in.
Flame Spread Index 15
15
ASTM E84
Oxygen Index 60 %
60 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 3.40e+15 ohm-cm
3.40e+15 ohm-cm
ASTM D257
Dielectric Constant 3.7

@Frequency 60 Hz
3.7

@Frequency 60 Hz
ASTM D150
Dielectric Strength 49.2 kV/mm
1250 kV/in
ASTM D147
Dissipation Factor 0.000070

@Frequency 1000 Hz
0.000070

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Cell Class 24446-B
ASTM D1784
Smoke Developed 70 to 125
ASTM E84