Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 48 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 48 g/10 min

@Load 2.16 kg,
Temperature 230 °C
48 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Network Polymers NPP 25-5001
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Melt Flow 48 g/10 min

@Pressure 0.655 MPa
48 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method
PolyOne Geon™ 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® 138 is a vinyl ester copolymer dispersion resin, exhibiting fast fusion at low processing temperatures, resulting in energy savings and the ability to work with heat sensitive substrates. The..
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Ineos ABS NOVODUR® L3FR ABS, Injection Grade  (discontinued **)
Injection molding grade, flame retardant, very easy flow. Contains no polyhalogenated diphenyls or diphenyl ethers.Applications: Television and computer housings.Information provided by the manufact..
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
LG Chemical HI153 ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Melt Flow 48 g/10 min

@Load 5.00 kg,
Temperature 260 °C
48 g/10 min

@Load 11.0 lb,
Temperature 500 °F
Calculated from MVR using melt density; ISO 1133
Lanxess Pocan® B 7425 000000 PBT, 20% Glass Spheres
PBT, 20% glass spheres, injection molding, low tendency to warp, improved surface finish
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
LG Chemical AF308 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi..
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 48 g/10 min

@Load 2.16 kg,
Temperature 250 °C
48 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Samyang Tribit® 1550GN30 PBT Alloy, Reinforced Flame Retardancy
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN30 is a reinforced, flame retardant (..
Melt Flow 48 g/10 min

@Load 2.16 kg,
Temperature 250 °C
48 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by..
Melt Flow 48 g/10 min
48 g/10 min
ISO 1133
Domo 2348TC Polypropylene Copolymer
Information provided by Domo.
Melt Flow 48 g/10 min
48 g/10 min
ISO 1133
Domo 2600TC Polypropylene Copolymer
Information provided by Domo.
Melt Flow 48 g/10 min

@Load 2.16 kg,
Temperature 190 °C
48 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Azoty Tarnow™ TARNOFORM 700 POM
Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade
High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali
Melt Flow 48 g/10 min

@Load 2.16 kg,
Temperature 190 °C
48 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer
IF33 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, good flexibility, ..
Melt Flow 48 g/10 min

@Load 2.16 kg,
Temperature 190 °C
48 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer
IN34 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, excellent flexibil..
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade
High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali
Melt Flow 48 g/10 min

@Load 2.16 kg,
Temperature 190 °C
48 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips LX8124 HDPE Injection Molding Resin  (discontinued **)
Resin Type: linear copolymer; ASTM D4976 Classification: PE 231, A 52600Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, excellent shrinkage resistanceApplic..
Copyright © lookpolymers.com All Rights Reserved