Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 46 g/10 min

@Load 10.0 kg,
Temperature 220 °C
46 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break 43.1 MPa
6250 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 56.9 MPa
8250 psi
50 mm/min; ASTM D638
Elongation at Break 23 %
23 %
50 mm/min; ASTM D638
Tensile Modulus 2.35 GPa
341 ksi
50 mm/min; ASTM D638
Flexural Strength 83.4 MPa
12100 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.35 GPa
341 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.37 J/cm

@Thickness 6.35 mm
2.57 ft-lb/in

@Thickness 0.250 in
ASTM D256
5.88 J/cm

@Thickness 3.17 mm
11.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C

@Thickness 6.40 mm
196 °F

@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C

@Thickness 6.40 mm
199 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 92.0 °C
198 °F
B/50; ISO R306
94.0 °C
201 °F
B/120; ISO R306
UL RTI, Electrical 85.0 °C
185 °F
UL RTI, Mechanical with Impact 85.0 °C
185 °F
UL RTI, Mechanical without Impact 85.0 °C
185 °F
Flammability, UL94 V-0

@Thickness 2.00 mm
V-0

@Thickness 0.0787 in
5VB

@Thickness 2.00 mm
5VB

@Thickness 0.0787 in