Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture

Category Polymer
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Pharmed®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features/Benefits:Outlasts silicone tubing in peristaltic pumps by up to 30 timesLow particulate spallationCan be autoclaved repeatedlyTemperature resistant from -60°F to 275°FWithstands repeated CIP and SIP cleaning and sterilizationFully tested to ISO 10993 standards to facilitate validation processMeets USP Class VI FDA and NSF criteriaTypical Applications include: Diagnostic test product manufacturing, cell harvest and media process systems, vaccine manufacturing, bioreactor process lines, production filtration and fermentation, sterile filling, shear sensitive fluid transfer.UL94-HB Flame Resistance Classification Passed. All data based on a 0.0625 inch test sample.(Available in multiple thicknesses.) Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792-91
Water Absorption 0.30 %
0.30 %
24 hours at 23°C; ASTM D570-81
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
Value given for 15 second test.; ASTM D2240-91
Tensile Strength, Yield 7.24 MPa
1050 psi
ASTM D-412-92
2.76 MPa

@Strain 100 %
400 psi

@Strain 100 %
ASTM D412-92
Elongation at Break 375 %
375 %
ASTM D-412-92
Tear Strength 22.4 kN/m
128 pli
Tear Resistance; ASTM D1004-93
Compression Set 32 %
32 %
Constant Deflection, Value given for test at 22 hrs, 70°C; ASTM D395-89 Method B
Tensile Set 47 %
47 %
ASTM D412-92
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Value given for heat resistance, not necessarily a recommended operating temperature.
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Brittleness Temperature -72.8 °C
-99.0 °F
ASTM D746-79
-40.0 °C
-40.0 °F
Low Temperature Flexibility; ASTM D412-92
Electrical Properties Metric English Comments
Dielectric Strength 24.0 kV/mm
610 kV/in
ASTM D149-93