Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -72.8 °C | -99.0 °F | ASTM D746-79 |
Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture Features/Benefits:Outlasts silicone tubing in peristaltic pumps by up to 30 timesLow particulate spallationCan be autoclaved repeatedlyTemperature resistant from -60°F to 275°FWithstands repea.. |
|||
Brittleness Temperature | -72.8 °C | -99.0 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE) DOWLEX™ IP-51 is an Improved Processing high density resin designed to offer excellent process-ability and impact performance. This resin was designed by optimization of the breadth, shape and pea.. |