Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D638 |
Multibase Multi-Pro® 0612 CW Polypropylene Calcium carbonate filler, 6% filer by weightForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D638 |
Multibase Multi-Pro® 2518 TU Polypropylene Talc Filled, 25% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Automotive Under the HoodInformation provided by Multibase |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D638 |
Multibase Multi-Pro® 4015 THW Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ DP 9052-3-1000 Polyethylene, High Density (HDPE) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D882 |
Formosa Plastics Formolene® LH5206 Injection Molding HDPE
(discontinued **) CopolymerApplications: Pails, lidsFormolene LH5206 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as specified in 2.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CM003P Polypropylene Impact Copolymer COPYLENE® CM003P is a fractional melt flow impact copolymer with a barefoot additive package which is specially formulated to excel in extrusion processes.Applications: Extrusion ProcessesInformati.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D638 |
Ineos R35C-02 Polypropylene Random Copolymer Grade R35C-02 is a high clarity, lubricated random copolymer with a high flow rate. This material is designed for high-speed injection molding of medium- to thin-walled parts requiring excellent cla.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D638 |
Techmer ES Electrablend® HDPE 04001 LE BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ESD Protection and ConductiveAppearance: BlackProcessing Method: ExtrusionInformation provided by .. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D638 |
Spartech PP5220 Calcium Carbonate Filled Homopolymer Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D-882 |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1700 Heat Bondable PTFE Film Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D-882 |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1900 Heat Bondable PTFE Film Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | ASTM Data |
Styron Magnum™ 213 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 6335N Impact Copolymer Polypropylene Impact Copolymer - Designed to Meet the Physical Requirements of Automotive Interior Trim Formolene® 6335N is an engineered, medium impact copolymer polypropylene. It was specifically developed to.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D638 |
Total PSI 740 Polystyrene Polystyrene 740 is an impact polystyrene designed for extrusion and injection molding. It is especially suitable for extrusion thermoforming applications requiring high glass and high stiffness, suc.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D638 |
Total HDPE BM961 High Density Polyethylene, High Gloss Blow Molding Resin Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | ASTM D638 |
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | ASTM D638 |
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin Resin Type: linear copolymerCharacteristics: excellent physical properties, medium molecular weight distribution, wide range of processing conditions, good flow for injection blow molding applicatio.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow UNIVAL™ DMDC-6400 NT 7 High Density Polyethylene Resin (HDPE) Excellent process-ability Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDC-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, wat.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | ASTM D638 |
Dow R792-35RNA Polypropylene Random Copolymer Resin OverviewControlled rheology productConsistent processabilityContains clarifying additiveContains an antistatic additiveComplies with U.S. FDA 21 CFR 177.1520 (c)3.1a, Canadian HPFB No ObjectionDOW R.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | |
Asahi Kasei Thermylene® P-40TC-8100 Chemically Coupled Polypropylene Compound, 40% Talc Filled Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D638 |
Asahi Kasei Thermofil P-40TC-1156 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | ASTM D638 |
Asahi Kasei Thermofil P-40TC-8100 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.6 MPa | 4300 psi | 2" per min, Type IV; ASTM D638 |
Amco PRIMATOP HDPE 055952 Injection Molding Polyethylene HDPE 055952 features maximum toughness, good top loading capability, and high surface gloss. Applications include pails and beverage crates.Former A-Top Polymers product; part of Amco product line s.. |