Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Fluran® F-5500-A Fluoroelastomer Tubing

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Fluran®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Fluran® F-5500-A Fluoroelastomer Tubing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluran® Severe Environment Tubing has the physical and chemical characteristics that make it ideal for severe environments, such as dry cleaning fluid lines and solvent recovery systems, where other flexible tubings fail. Fluran® Severe Environment Tubing can be used in continuous service with temperatures as high as 400°F (204°C) and has excellent resistance to corrosive chemicals, oils, fuels, solvents and most mineral acids.
Physical Properties Metric English Comments
Specific Gravity 1.90 g/cc
1.90 g/cc
ASTM D792
Water Absorption 0.23 %
0.23 %
24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
15 sec.; ASTM D2240-02
Tensile Strength, Ultimate 9.65 MPa
1400 psi
ASTM D412-98
Elongation at Break 300 %
300 %
ASTM D412-98
100% Modulus 0.00241 GPa
0.350 ksi
ASTM D412-98
Tear Strength 17.5 kN/m
99.9 pli
ASTM D1004-94
Compression Set 37 %

@Temperature 70.0 °C
37 %

@Temperature 158 °F
22 hrs.; ASTM D395-02 Method B
Tensile Set 13 %
13 %
ASTM D412-98
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746-98
Electrical Properties Metric English Comments
Dielectric Strength 19.7 kV/mm
500 kV/in
ASTM D149-97
Descriptive Properties Value Comments