Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brittleness Temperature = -51.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable L00221 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Brittleness Temperature -51.0 °C
-59.8 °F
Low temp embrittlement; ASTM D746
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
Brittleness Temperature -51.0 °C
-59.8 °F
Low temp embrittlement; ASTM D746
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746-98
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746-98
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Contains PET film reinforcement. Standard available  thickness 0.064"Features and Benefits of PORON Products: Excelle..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746-98
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746-98
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746-98
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Brittleness Temperature -51.0 °C
-59.8 °F
Low temp embrittlement; ASTM D746
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4..
Brittleness Temperature <= -51.0 °C
<= -59.8 °F
TPE-0089 (ASTM D 746)
Advanced Elastomer Systems Santoprene® 253-36 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746-98
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab..
Brittleness Temperature -51.0 °C
-59.8 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TCP Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746
Teknor Apex APEX® 121 Polyvinyl Chloride, Flexible
Notes: 90°C Jacket; RoHS Compliant Features: Good UV Resistance Uses: Telephone Drop Wire Insulation; Telephone Drop Wire JacketingAgency Ratings: REA Unspecified Rating Forms: PelletsInformation..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746
Teknor Apex Flexalloy® 9800-45 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746
Teknor Apex Flexalloy® 9800-50 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MW Uses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746
Teknor Apex Flexalloy® 9800-55 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746
Teknor Apex Flexalloy® 9800-60 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
Brittleness Temperature -51.0 °C
-59.8 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TCP Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746
Teknor Apex Telcar® TL-1402G Thermoplastic Elastomer
Notes: Non-halogenated, Flame Retardant TPE; RoHS Compliant Uses: Connectors; Electrical/Electronic Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injec..
Brittleness Temperature -51.0 °C
-59.8 °F
AlphaGary Garaflex™ E 4762 A1 LCF Vinyl Thermoplastic Elastomer
Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable105°C rated low temperature flexible booster cable jacket application
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D-746
Axiall 18760 Wire & Cable Flexible PVC
Non-lead stabilized, matte-finish, jacketing compound with excellent low temperature performance. Maximum 105°C service temperature at 40+ mil. Ideally suited for 90°C applications.Information p..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746-98
Saint-Gobain Fluran® F-5500-A Fluoroelastomer Tubing
Fluran® Severe Environment Tubing has the physical and chemical characteristics that make it ideal for severe environments, such as dry cleaning fluid lines and solvent recovery systems, where othe..
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746
Eastman D4041-P Polyethylene  (discontinued **)
Low-density polyethylene D4041-P is a recommended for use in the boardstock coating industry for applications such as breadboard, cupstock, and liquid packaging board. This resin has low neck-in an..
Brittleness Temperature -51.0 - -12.0 °C
-59.8 - 10.4 °F
Average value: -36.5 °C Grade Count:24
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..
Copyright © lookpolymers.com All Rights Reserved