Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond LED401LV One Component, Moderate Viscosity LED Curable System

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond LED401LV One Component, Moderate Viscosity LED Curable System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond LED401LV is a very special, one part LED type system that will cure when exposed to a light source emitting 405 nm wavelength and where the presence of any UV light is minimal or incidental. When exposed to the light, LED401LV will cure completely tack-free in sections of 1/8 inch thick and beyond. The system can be used as an adhesive, sealant, coating and encapsulant. It has excellent optical clarity and light transmission properties, even with a very slight amber tint. Prior to cure, it has a moderate viscosity consistency, but it remains flowable. Additionally, the formulation is solvent-free.
Physical Properties Metric English Comments
Viscosity 60000 - 80000 cP
60000 - 80000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D >= 65
>= 65
Tensile Strength >= 17.2 MPa
>= 2500 psi
Tensile Modulus 0.172 - 0.345 GPa
25.0 - 50.0 ksi
Thermal Properties Metric English Comments
CTE, linear 65.0 - 70.0 µm/m-°C
36.1 - 38.9 µin/in-°F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Glass Transition Temp, Tg 60.0 - 65.0 °C
140 - 149 °F
Optical Properties Metric English Comments
Transmission, Visible >= 90 %
>= 90 %
thickness not specified
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Constant 3.9

@Frequency 60.0 Hz
3.9

@Frequency 60.0 Hz
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
unopened containers with no exposure to light, with no exposure to light
Descriptive Properties Value Comments
Color Clear
Users viewing this material also viewed the following: