Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | |
P & P Technology Conductive Elastomer Nickel Graphite particlesInformation provided by P & P Technology |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Parker Chomerics Tecknit® 0236 Conductive Silicone Sealant/Adhesive Comments: Thick flexible pasteTypical Applications: Bonding Ag/Al elastomerInformation provided by Chomerics |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 4806 UP Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 8601 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 8602 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group SURAPLAST 54 UPA Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ASTM D792 |
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ASTM D792 |
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | ASTM D297 |
Greene Tweed FPD Blueâ„¢ 707 Fluoroelastomer Specifically developed for flat panel display CVD and dry plasma etch equipment where seal reliability and minimal contamination are essential, FPD Blueâ„¢ 707 fluoroelastomer provides excellent .. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | ASTM D-792 |
Glastic T-160 Fiberglass-Reinforced Polyester Laminate Grade T-160 is a new, high-strength, heat-resistant laminate. This highly creep-resistant material is excellent for applications where electrically insulating materials are subject to physical load.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber. |
|||
Specific Gravity | 1.90 - 1.98 g/cc | 1.90 - 1.98 g/cc | ASTM D792 |
Adamas Adalon® 403 PTFE, 15% Polyimide Information provided by Adamas, HPM |
|||
Specific Gravity | 1.90 - 1.96 g/cc | 1.90 - 1.96 g/cc | |
3M Dyneon™ FX 5912 Dynamar™ Polymer Processing Additive Dynamar FX 5912 is a free-flowing fluorothermoplastic processing aid that is designed for use at very low levels to improve the processing of thermoplastics. Typical use levels of 200 to 1000 ppm ha.. |
|||
Specific Gravity | 1.90 - 2.05 g/cc | 1.90 - 2.05 g/cc | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Specific Gravity | 1.90 - 1.93 g/cc | 1.90 - 1.93 g/cc | ASTM D792 |
Adamas Adalon® 410 PTFE+ PEEK Information provided by Adamas, HPM |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
3M Dyneon™ FE 5830Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5830Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | |
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | ASTM D792 |
Saint-Gobain Fluran® F-5500-A Fluoroelastomer Tubing Fluran® Severe Environment Tubing has the physical and chemical characteristics that make it ideal for severe environments, such as dry cleaning fluid lines and solvent recovery systems, where othe.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Parker Chomerics CHO-BOND 2166 Part B Silicone Information provided by Chomerics |