Material Notes:
Excellent for light dynamic and static service; Limited wear and heat resistance; Low gas permeability; Good cryogenic properties; Moderate to hard vacuum service; FDA approved. Information provided by Saint-Gobain Performance Plastics.
Physical Properties Metric English Comments
Density 2.16 g/cc
0.0780 lb/in³
ASTM D792
Deformation 10 %

@Time 86400 sec
10 %

@Time 24.0 hour
13.8 MPa (2000 psi) load; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 50 - 65
50 - 65
ASTM D2240
Tensile Strength 27.5 MPa
3990 psi
ASTM D1708
Elongation at Break 300 %
300 %
ASTM D1708
Tensile Modulus 0.386 GPa
56.0 ksi
ASTM D638
Compressive Yield Strength 8.27 MPa

@Strain 1.00 %
1200 psi

@Strain 1.00 %
ASTM D695
Compressive Modulus 0.558 GPa
80.9 ksi
ASTM D695
Coefficient of Friction 0.05 - 0.08
0.05 - 0.08
ASTM D3702
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 130 µm/m-°C

@Temperature 26.0 - 200 °C
72.2 µin/in-°F

@Temperature 78.8 - 392 °F
Mold Direction; ASTM D696
CTE, linear, Transverse to Flow 152 µm/m-°C

@Temperature 26.0 - 200 °C
84.4 µin/in-°F

@Temperature 78.8 - 392 °F
ASTM D696
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -268 °C
-450 °F
Descriptive Properties Value Comments
Color White