Polymer Property : Compressive Yield Strength = 8.27 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 8.27 MPa
1200 psi
TM R050-38
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11..
Compressive Yield Strength 8.27 MPa
1200 psi
TM R050-38
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP1112NC Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Black is a modified version of the standard EP11..
Compressive Yield Strength 8.27 MPa
1200 psi
Max load under tribological use
Saint-Gobain Rulon® XL Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Compressive Yield Strength 8.27 MPa

@Strain 1.00 %
1200 psi

@Strain 1.00 %
ASTM D695
Saint-Gobain Fluoroloy® A01 High Performance Seal Material
Excellent for light dynamic and static service; Limited wear and heat resistance; Low gas permeability; Good cryogenic properties; Moderate to hard vacuum service; FDA approved. Information provide..
Compressive Yield Strength 8.27 MPa
1200 psi
Stabilized, typ
Hexcel® HexWeb® CR III 1/8-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Yield Strength >= 8.27 MPa
>= 1200 psi
Bare, min
Hexcel® HexWeb® CR III 1/8-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Yield Strength 8.27 MPa
1200 psi
Stabilized, typ
Hexcel® HexWeb® CR-PAA™ 1/8-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Compressive Yield Strength >= 8.27 MPa
>= 1200 psi
Bare, min
Hexcel® HexWeb® CR-PAA™ 1/8-5056-0.002 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Compressive Yield Strength 8.27 - 440 MPa
1200 - 63800 psi
Average value: 98.9 MPa Grade Count:5
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..
Compressive Yield Strength >= 8.27 MPa
>= 1200 psi
Stabilized, min
Hexcel® HexWeb® CR III 1/16-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..