Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -268 - -200 °C | -450 - -328 °F | Average value: -215 °C Grade Count:19 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
Minimum Service Temperature, Air | -268 - -20.0 °C | -450 - -4.00 °F | Average value: -171 °C Grade Count:29 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3500 PTFE Gasketing, Silica Filler PTFE with silica filler.Improved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE sheetsExcellent bolt torque r.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3502 PTFE Gasketing, Silica Filler, Oxygen Service PTFE with silica filler - Oxygen serviceImproved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE sheetsExcelle.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3503 PTFE Gasketing, Barium Sulfate Filler, Oxygen Service PTFE with barium sulfate filler - Oxygen service.Improved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE shee.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3535 PTFE Joint Sealant Pure PTFE is chemically inert, withstands a wide range of chemicalsConforms to FDA regulationsInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3540 Microcellular PTFE Gasketing Microcellular PTFE.Highly compressible PTFE seals under low bolt load- suitable for many non-metallic flangesCompressible material conforms to surface irregularities, especially on warped, pitted or.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3545 Layered Microcellular PTFE Gasketing Microcellular PTFE gasket with rigid PTFE coreHighly compressible PTFE outer layers seal under low bolt load- suitable for many non-metallic flangesCompressible layers conform to surface irregularit.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3565 ENVELON® PTFE Gasketing, Glass Microsphere Filled PTFE with aluminosilicate microsphere filler.Soft, deformable exterior conforms to surface irregularities; ideal for worn, warped or pitted flangesStable blue core improves cold flow resistanceLow b.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3594 PTFE Gasketing, Glass Fiber Filled PTFE with glass fiber fillerInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Fluoroloy® A12 High Performance Seal Material Excellent wear and heat resistance; Non-abrasive; Recommended for moderate to high speed service running against soft or hard metals; Performs well against lubricated and non-lubricated surfacesInfo.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Fluoroloy® A16 High Performance Seal Material General purpose material for heat and wear resistance; Recommended for dry and poorly lubricated applications; Particularly suitable for water and steam service
Information provided by Saint-Goba.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Fluoroloy® A01 High Performance Seal Material Excellent for light dynamic and static service; Limited wear and heat resistance; Low gas permeability; Good cryogenic properties; Moderate to hard vacuum service; FDA approved.
Information provide.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Fluoroloy® A08 High Performance Seal Material Superior heat and wear resistance; Recommended for moderate to high speed dynamic service running against soft metals; Non-abrasive
Information provided by Saint-Gobain Performance Plastics. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
W. L. Gore GORE™ 800 PTFE Universal Pipe Gasket (Style 800) 100% expanded PTFE, with multi-directional strength. Resistant to all media in the 0-14 pH range, except molten alkali metals and element fluorine, particularly at elevated temperatures and pressure.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Garlock GYLON® 3505 PTFE Gasketing, Glass Microsphere Filled PTFE with aluminosilicate microspheres - NSF 61 approved (drinking water) - Oxygen serviceImproved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems.. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Fluoroloy® A30 High Performance PTFE/Glass Seal Material Excellent heat, wear, and chemical resistance; Good cryogenic properties; Can be abrasive running against soft metals at high surface speed; Excellent material for back-up rings
Information .. |
|||
Minimum Service Temperature, Air | -268 °C | -450 °F | |
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f.. |