Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 8.27 MPa | 1200 psi | TM R050-38 |
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11.. |
|||
Compressive Yield Strength | 8.27 MPa | 1200 psi | TM R050-38 |
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Black is a modified version of the standard EP11.. |
|||
Compressive Yield Strength | 8.27 MPa | 1200 psi | Max load under tribological use |
Saint-Gobain Rulon® XL Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Compressive Yield Strength | 8.27 MPa @Strain 1.00 % |
1200 psi @Strain 1.00 % |
ASTM D695 |
Saint-Gobain Fluoroloy® A01 High Performance Seal Material Excellent for light dynamic and static service; Limited wear and heat resistance; Low gas permeability; Good cryogenic properties; Moderate to hard vacuum service; FDA approved.
Information provide.. |
|||
Compressive Yield Strength | 8.27 MPa | 1200 psi | Stabilized, typ |
Hexcel® HexWeb® CR III 1/8-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Yield Strength | >= 8.27 MPa | >= 1200 psi | Bare, min |
Hexcel® HexWeb® CR III 1/8-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Yield Strength | 8.27 MPa | 1200 psi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 1/8-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Yield Strength | >= 8.27 MPa | >= 1200 psi | Bare, min |
Hexcel® HexWeb® CR-PAA™ 1/8-5056-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Yield Strength | 8.27 - 440 MPa | 1200 - 63800 psi | Average value: 98.9 MPa Grade Count:5 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Compressive Yield Strength | >= 8.27 MPa | >= 1200 psi | Stabilized, min |
Hexcel® HexWeb® CR III 1/16-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |