Material Notes:
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Water Absorption 0.80 %
0.80 %
24 hour; ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 220 °C
18 g/10 min

@Load 4.76 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 30
30
ASTM D2240
Tensile Strength, Ultimate 21.6 MPa
3130 psi
ASTM D638
Tensile Strength, Yield 0.588 MPa

@Strain 5.00 %
85.3 psi

@Strain 5.00 %
ASTM D638
1.77 MPa

@Strain 10.0 %
256 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
Flexural Modulus 0.0275 GPa
3.98 ksi
ASTM D790
Resilience 72
72
ASTM D2632
Izod Impact, Notched NB
NB
ASTM D256
Tear Strength 95.0 kN/m
542 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 174 °C
345 °F
ASTM D3418