Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 542 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 95.0 kN/m
542 pli
ISO 34B
Huntsman AVALON® 80 ABU Thermoplastic Polyurethane
Introduction: AVALON 80 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABU is part of the AVALON Perform Range and offers a premi..
Tear Strength 95.0 kN/m
542 pli
Huntsman IROGRAN® A 95 K 6977 TPU-For Seals
Information provided by Huntsman
Tear Strength 95.0 kN/m
542 pli
ISO 34-1B
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as..
Tear Strength 95.0 kN/m
542 pli
ISO 34B
Huntsman AVALON® 80 AB Thermoplastic Polyurethane
Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma..
Tear Strength 95.0 kN/m
542 pli
ISO 34B
Huntsman AVALON® 90 AHT DP Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
Tear Strength 95.0 kN/m
542 pli
ASTM D624
GRECO ISOTHANE 1090A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tear Strength 95.0 kN/m
542 pli
Die B
Momentive Performance Materials FQE207U Heat Cured Fluorosilicone Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 95.0 kN/m
542 pli
ASTM D1004
SK Chemicals SKYPEL P147D Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tear Strength 95.0 kN/m
542 pli
ASTM D1004
SK Chemicals SKYPEL G130D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tear Strength 95.0 kN/m
542 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-A895 Aliphatic TPU
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 95.0 kN/m
542 pli
with incision; ISO 34B
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 95.0 kN/m
542 pli
without incision; ISO 34B
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Tear Strength 95.0 kN/m
542 pli
with incision; ISO 34B
Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 95.0 kN/m
542 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-1485RV Polyester Based TPU
Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 95.0 kN/m
542 pli
DIN 53515
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 95.0 kN/m
542 pli
ISO 34
Chengdu Polyster H4040 Thermoplastic Polyether-ester Elastomer (TPEE)
Low modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent flex resistance, especially at low temperatures. Moldable even in thin sections. Can be used in light..
Tear Strength 95.0 kN/m
542 pli
unnotched; ASTM D624 (C)
Arkema Group Pebax® 4033 Polyether Block Amide (PEBA)
Typical application: Mechanical partsInformation provided by Arkema Group
Tear Strength 95.0 kN/m
542 pli
ASTM D624
C.O.I.M. LARIPUR® LPR8520 Standard Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Tear Strength 95.0 kN/m
542 pli
ASTM D624
BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..
Tear Strength >= 95.0 kN/m
>= 542 pli
ISO 34
Austin Novel Materials Texalan® 390A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tear Strength >= 95.0 kN/m
>= 542 pli
ISO 34
Austin Novel Materials Texalan® 495A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tear Strength >= 95.0 kN/m
>= 542 pli
ISO 34
Austin Novel Materials Texalan® 585A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tear Strength >= 95.0 kN/m
>= 542 pli
ISO 34
Austin Novel Materials Texalan® 764D PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tear Strength 95.0 kN/m
542 pli
ASTM D624
C.O.I.M. LARIPUR® LPR8025 Special Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Tear Strength 95.0 kN/m
542 pli
DIN ISO 34-1/Bb
BASF Elastollan S 90 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tear Strength >= 95.0 kN/m
>= 542 pli
ISO 34
Austin Novel Materials Texalan® 695A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tear Strength 95.0 kN/m
542 pli
with incision; ISO 34B
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Copyright © lookpolymers.com All Rights Reserved