Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 21.6 MPa | 3130 psi | 500mm/min; ASTM D638 |
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural Film, Shoe solesCSA No. 24937-78-8Information provided by LG Chemical |
|||
Tensile Strength, Ultimate | 21.6 MPa | 3130 psi | ASTM D638 |
KKPC Kuhmo HI 425EP Extrusion Molding HIPS Common Uses: Refrigerator inner liners, door liners, disposable cups, food packaging sheet, wrapping films, trays, washing machinesHIPS is a functional resin made by copolymerization of styrene mono.. |
|||
Tensile Strength, Ultimate | >= 21.6 MPa @Temperature 100 °C |
>= 3130 psi @Temperature 212 °F |
|
Sibur SKI-3 Superior Quality, 1st Group Isoprene Rubber (IR) Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. For production of tires and rubber technical articles of wide assortment. |
|||
Tensile Strength, Ultimate | >= 21.6 MPa @Temperature 100 °C |
>= 3130 psi @Temperature 212 °F |
|
Sibur SKI-3 Superior Quality, 2nd Group Isoprene Rubber (IR) Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. For production of tires and rubber technical articles of wide assortment. |
|||
Tensile Strength, Ultimate | 21.6 MPa | 3130 psi | ASTM D638 |
SK Chemicals SKYTHANE® SG200 SKYGREEN Biodegradable Thermoplastic SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been develo.. |
|||
Tensile Strength, Ultimate | >= 21.6 MPa @Temperature 100 °C |
>= 3130 psi @Temperature 212 °F |
|
Sibur SKI-3S Superior Quality, 1st Group Isoprene Rubber (IR) Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. It is used instead of natural rubber during production of colored rubber articles, medical articles, and rubbers contacting with food products. |
|||
Tensile Strength, Ultimate | >= 21.6 MPa @Temperature 100 °C |
>= 3130 psi @Temperature 212 °F |
|
Sibur SKI-3S Superior Quality, 2nd Group Isoprene Rubber (IR) Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. It is used instead of natural rubber during production of colored rubber articles, medical articles, and rubbers contacting with food products. |
|||
Tensile Strength, Ultimate | 21.6 MPa | 3130 psi | ASTM D638 |
SK Chemicals SKYPEL G130D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tensile Strength, Ultimate | 21.6 MPa | 3130 psi | ASTM D412 |
Lubrizol Estane® T465A Thermoplastic Polyurethane Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |
|||
Tensile Strength, Ultimate | 21.6 MPa @Treatment Temp. 150 °C, Time 605000 sec |
3130 psi @Treatment Temp. 302 °F, Time 168 hour |
Heat Aging; ASTM D 412/ASTM D 573 |
Zylog Neoplast® 240 FT EB Thermoplastic Vulcanizate Neoplast 240 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Tensile Strength, Ultimate | 21.6 MPa | 3130 psi | ASTM D412 |
Lubrizol Estane® CR185A Thermoplastic Polyurethane Type: Estane® CR185A is a Shore 85A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |