S&E Specialty Polymers TufFill™ 5000-SN4 PP, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer S&E Specialty Polymers
Trade Name TufFill™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFill™ 5000-SN4 PP, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: A No Bloom, UL 94 V-0 Polypropylene Compound TufFill™ 5000SN series is a specially engineered, low bloom, flame retardant polypropylene compound designed with halogen based technology. TufFill™ 5000SN series exhibits a balance of high flexural modulus and good impact. It is designed for extrusion applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 29.6 MPa
>= 4300 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
Ultimate; ASTM D638
Flexural Modulus 3.59 GPa
521 ksi
tangent; ASTM D790
Flexural Modulus, 1% Secant 2830 MPa
410000 psi
ASTM D790
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
ASTM D256
Dart Drop Total Energy 8.54 J/cm
0.0160 ft-lb/mil
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 126.5 °C

@Thickness 3213 mm
259.7 °F

@Thickness 126.5 in
0.125; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.1 °C

@Thickness 3.17 mm
153 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
Oxygen Index >= 25.0 %
>= 25.0 %
ASTM D2863
Processing Properties Metric English Comments
Processing Temperature 193 - 210 °C
380 - 410 °F
Profile
210 °C
410 °F
Stock