Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
NYCOA 2037 15% Glass Filled Nylon 6 15% glass filled very high viscosity nylon 6Information provided by NYCOA, Inc. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | Tangent; ASTM D790 |
RheTech Products F36-01 35% Mica Reinforced Polypropylene Copolymer, Black Applications: Cowl screensHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | Tangent; ASTM D790 |
RheTech Products G20P100-01UV 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: Rigid exterior componentsHousingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | ASTM D790 |
PolyOne Maxxam™ PPH-20G Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | tangent; ASTM D790 |
S&E Specialty Polymers TufFill™ 5000-SN4 PP, Flame Retardant Application: A No Bloom, UL 94 V-0 Polypropylene Compound TufFill™ 5000SN series is a specially engineered, low bloom, flame retardant polypropylene compound designed with halogen based technology... |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP FARADEX NX96302 PC+ABS LNP* FARADEX* NX96302 is a compound based on PC+ABS resin containing Stainless Steel Fibers. |
|||
Flexural Modulus | 3.59 - 29.0 GPa | 520 - 4210 ksi | Average value: 11.7 GPa Grade Count:50 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Global GAB-105 5% Glass Reinforced ABS Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Techmer ES Electrablend® PEI 04001 MB Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp DF002L PC LNP THERMOCOMP* DF002L is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC-IP for the America.. |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EM7301HF PPE+PS (Asia Pacific) Easy flow, 10% glass filled, improved adhesion PPO/HIPS alloy. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Teknor Apex Sinpolene GPP1620 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 20% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Chase Plastics CP Pryme® N120GL (COND, 50% RH) Nylon 6, 20% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Ecomass® 1005ZD96 Tungsten Powder Filled Co-Polyamide, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Co-Polyamide (COPA), Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing .. |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | ISO 178 |
Ecomass® 1007ZC85 Stainless Steel Filled COPA Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsStainless Steel Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Poly.. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Ensinger XP-150 Compression Molded Polyimide Unfilled, Premium Grade The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st.. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FG-0659 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FG-2153R 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FM-Y249B 30% Glass/Mineral Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | |
Asahi Kasei Xyron® G701H Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Asahi Kasei Thermofil P-40TC-0158 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.59 - 8.20 GPa | 521 - 1190 ksi | Average value: 5.46 GPa Grade Count:7 |
Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Glass/Graphite Reinforced". Each property range of values reported is minimum and m.. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | Tangent; ASTM D790 |
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | Tangent; ASTM D790 |
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |