SCG Chemicals EL-Leneâ„¢ M3504DXP Octene (C8) Rotational Molding Resin

Category Polymer , Thermoplastic
Manufacturer SCG Chemicals Co.
Trade Name EL-Lene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Leneâ„¢ M3504DXP Octene (C8) Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Natural base resin available in powder formKey Characteristics:Excellent ESCRExcellent impact resistanceLow warpageFair processingTypical Applications: Chemical storage tanks, diesel tanks, spray tanks, IBC, and marine productsInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.935 g/cc
0.935 g/cc
ASTM D1505
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM D638
Elongation at Break 1100 %
1100 %
ASTM D368
Flexural Modulus 0.650 GPa
94.3 ksi
ASTM D790
Dart Drop Total Energy 2.30 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00431 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
Thermal Properties Metric English Comments
Melting Point 125 °C
257 °F
ASTM D2117
Crystallization Temperature 105 °C
221 °F
ASTM D2117
Descriptive Properties Value Comments
Food Contact Approved FDA and AS/NZS 4020
Heavy Metal Free (Base Resin) Yes
Peak Internal Air Temperature 225°C
TPE Method
Shrinkage Level very small
TPE Method
UV Stabilizer UV-6 &UV-8
ASTM G155