Polymer Property : Dart Drop Total Energy = 0.00431 ft-lb/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Total Energy 2.30 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00431 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
SCG Chemicals EL-Leneâ„¢ M3504DXP Octene (C8) Rotational Molding Resin
Natural base resin available in powder formKey Characteristics:Excellent ESCRExcellent impact resistanceLow warpageFair processingTypical Applications: Chemical storage tanks, diesel tanks, spray t..
Dart Drop Total Energy 2.30 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00431 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
SCG Chemicals EL-Lene™ M50 Octene (C8) Rotational Molding Resin
Color compound resin available in pellet / powder formKey Characteristics:Excellent ESCRExcellent impact resistanceLow warpageFair processingTypical Applications: Chemical storage tanks, diesel tan..