Material Notes:
CAPILENE® T 50 is a high melt flow rate homopolymer for injection molding characterized by good flow properties combined with good stiffness. APPLICATIONS CAPILENE ® T 50 is recommended for injection molding of household articles, closures, crates, containers and garden furniture.
Physical Properties Metric English Comments
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 0.230 J/cm

@Temperature >=23.0 °C
0.431 ft-lb/in

@Temperature >=73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
ASTM D648
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ASTM D1525
Users viewing this material also viewed the following: