Material Notes:
This product is suitable for airbag enclosures and is based on polyolefins/kraton rubber, exhibiting good paintability and low temperature performance.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792-91
Melt Flow 2.0 g/10 min
2.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 14.5 MPa
2100 psi
20" / min.; ASTM D-683-95
Elongation at Break >= 1300 %
>= 1300 %
ASTM D638-95
Flexural Modulus 0.2345 GPa
34.01 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Gardner Impact 18.1 J
13.3 ft-lb
No break; ASTM D5420-95
Thermal Properties Metric English Comments
Melting Point 138 °C
280 °F
Glass Transition Temp, Tg -35.0 °C
-31.0 °F