Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Water Absorption 0.050 %

@Time 173000 sec
0.050 %

@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ASTM D955
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
17 g/10 min

@Load 5.00 kg,
Temperature 210 °C
17 g/10 min

@Load 11.0 lb,
Temperature 410 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
30S reading; ASTM D2240
Tensile Strength at Break 4.00 MPa
580 psi
50 mm/min; ISO 527
5.00 MPa
725 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break >= 400 %
>= 400 %
Type I, 50 mm/min; ASTM D638
>= 400 %
>= 400 %
50 mm/min; ISO 527
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.0500 GPa
7.25 ksi
12.5 mm/min; ISO 178
Tear Strength 46.0 kN/m
262 pli
ISO 6383
Thermal Properties Metric English Comments
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 1.70e+16 ohm-cm
1.70e+16 ohm-cm
IEC 60093
Dielectric Constant 2.4

@Frequency 1.00e+6 Hz
2.4

@Frequency 1.00e+6 Hz
IEC 60250
2.4

@Frequency 50.0 - 60.0 Hz
2.4

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 26.0 kV/mm

@Thickness 2.00 mm
660 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.00050

@Frequency 1.00e+6 Hz
0.00050

@Frequency 1.00e+6 Hz
IEC 60250
0.037

@Frequency 50.0 - 60.0 Hz
0.037

@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Users viewing this material also viewed the following: