Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.00 MPa | 580 psi | ISO 37 |
PolyOne OnFlex™ S EH 40A-3S7001 Thermoplastic Elastomer (TPE) OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | ISO 37 |
PolyOne OnFlex™ S EH 50A-3S7002 Thermoplastic Elastomer (TPE) OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | ISO 37 |
PolyOne OnFlex™ S HF 70A-3S1984 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | After Curing |
Silikony Polskie Gumosil WW Silicone Rubber Flexible with good tearing resistance |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4145 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4145 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | ASTM D638 |
ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | ASTM D638 |
ELASTO UK Dryflex® 402701S SBS Based Material, 70A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | ASTM D412 and ISO 37 |
ExxonMobil Exact™ 9071 Ethylene-based Plastomer Resin Product Description: Exact 9071 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-50E500 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has controlled rheology for robotic or specialty extrusion applications. This g.. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 8221-55M300 Thermoplastic Vulcanizate - UV Resistant Product Description: A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requ.. |
|||
Tensile Strength at Break | >= 4.00 MPa | >= 580 psi | ISO R 527 |
Fainplast Compounds CRKA 78 Flexible PVC, Flame Retardant Electrical Bedding Lead Free Flame retardant bedding |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | ASTM D412 |
3M 560 Polyurethane Adhesive Sealant 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX E 50.1 TPE-V, Shore A50 TPE-VInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | 4.00 MPa | 580 psi | ASTM D638 |
Arkema Group EVATANE® 18-500 Copolymer Ethylene - Vinyl Acetate EVATANE® 18-500 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 18-500 is stabilized with antioxidants. The High Vinyl Acetate .. |
|||
Tensile Strength at Break | 4.00 - 6.00 MPa | 580 - 870 psi | DIN 53504 S2 |
Wacker Silicones Geniomer® 80 Silicone TPE SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Tensile Strength at Break | 4.00 - 5.50 MPa | 580 - 798 psi | DIN 53504 S2 |
Wacker Silicones Geniomer® 60 Silicone TPE SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |