Polymer Property : Linear Mold Shrinkage, Flow = 0.0048 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics NORYL WCP700 PPE-TPE
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Linear Mold Shrinkage, Flow 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Asia Pacific)
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Linear Mold Shrinkage, Flow 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Europe-Africa-Middle East)
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Linear Mold Shrinkage, Flow 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics NORYL WCP821 PPE-TPE
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Linear Mold Shrinkage, Flow 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Asia Pacific)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Linear Mold Shrinkage, Flow 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Linear Mold Shrinkage, Flow 0.0048 cm/cm
0.0048 in/in
60x60x2mm; ISO 294
BASF Ultradur B 4300 G4 High Speed Unc. 20% Glass Filled PBT
Ultradur B 4300 G4 High Speed Unc. is a high flow, fast cycling with low warpage, 20% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap..
Linear Mold Shrinkage, Flow 0.0048 cm/cm
0.0048 in/in
ISO 2577
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Conditioned)
Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el..
Linear Mold Shrinkage, Flow 0.0048 cm/cm
0.0048 in/in
ISO 2577
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry)
Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el..