SABIC Innovative Plastics NORYL GTX GTX6009 PPE+PS+PA6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX GTX6009 PPE+PS+PA6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PA6 based unfilled GTX for Wheel cover
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.012 - 0.013 cm/cm

@Thickness 3.20 mm
0.012 - 0.013 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 55.0 MPa
7980 psi
SABIC - Japan Method
Elongation at Break 180 %
180 %
SABIC - Japan Method
Flexural Strength 84.0 MPa
12200 psi
ASTM D790
Flexural Modulus 2.15 GPa
312 ksi
ASTM D790
Izod Impact, Notched 7.25 J/cm
13.6 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.9 - 44.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 160 °C

@Thickness 3.20 mm
320 °F

@Thickness 0.126 in
unannealed; ASTM D648