Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ASTM D955 |
PolyOne Maxxam™ PPH-20C Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.013 cm/cm | 0.0080 - 0.013 in/in | ASTM D955 |
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO 294-4 |
Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.013 cm/cm | 0.0060 - 0.013 in/in | ASTM D955 |
PolyOne Dynalloy™ OBC 8100-N75 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N75 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | 0.125"x0.5"x5" bar; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Thickness 3.20 mm |
0.011 - 0.013 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HI5302A PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | |
LATI Laticonther 52/35 CP1/45 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RAL22 is a compound based on PA66 resin containing PTFE, Aramid Fiber. Added Features: Internally Lubricated |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.013 cm/cm | 0.012 - 0.013 in/in | mold temp=60°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.013 cm/cm | 0.012 - 0.013 in/in | mold temp=60°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Thickness 3.20 mm |
0.011 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX905 PPE+PS+PA Automotive. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Thickness 3.20 mm |
0.011 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA (Asia Pacific) Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Thickness 3.20 mm |
0.011 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX917 PPE+PS+PA This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.013 cm/cm @Thickness 3.20 mm |
0.010 - 0.013 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.013 cm/cm | 0.0070 - 0.013 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Time 86400 sec |
0.011 - 0.013 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ASTM D955 |
Chase Plastics CP Pryme® N100HL (Dry) Nylon 6, Heat Stabilized, Lubricated Features: Heat stabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1599-BK Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1599-BK11 Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1599-GY Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Thickness 4.00 mm |
0.011 - 0.013 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide 6 80E10 PA6, Injection Molded Staramide 6 80E10 is a high density, Polyamide 6, Injection Molding Resin (also known as 680E10)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.013 cm/cm @Thickness 4.00 mm |
0.011 - 0.013 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide RB004 PA66, 20% Glass Bead Filled, Injection Molded Staramide RB004 is a 20% Glass Bead Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0105 - 0.013 cm/cm | 0.0105 - 0.013 in/in | |
LATI Latilub 95-15T PSU, PTFE Filled Self-lubricating product based on Polysulfone (PSU). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |