Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.15 GPa | 312 ksi | Tangent (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 808 C3WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Asia Pacific) Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1483T PC Copolymer Lexan* EXL1483T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release, transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility i.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Europe-Africa-Middle East) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) .. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE9925A PC (Asia Pacific) Illuminate / edge glow color effect grade of Lexan 9925A. 9925A is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR .. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2mm/min; ASTM D790 |
Kingfa HIPS-5197 High Impact Polystyrene Features:UL 94 HB @ 1.6mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientsApplications:Injection moldingGas assistant moldingTV & Audio housingElec.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp DP003F PC LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 308 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 309 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500. Available in Natural (1001) only. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS (Asia Pacific) LNP* Stat-loy* N30009 is a compound based on PC+ABS Blend resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY NX03583 PC+ABS (Asia Pacific) LNP STAT-LOY* NX03583 is a compound based on PC+ABS Blend resin containing Anti-Static, Flame Retardant. Added features of this material include: Antistat. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Asia Pacific) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the A.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Asia Pacific) PPE/PS, 80degC, FR V-0, high flow |
|||
Flexural Modulus | 2.15 GPa @Temperature 90.0 °C |
312 ksi @Temperature 194 °F |
ASTM D790 |
LATI LARIL 13 Light Brown Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the E.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
Teknor Apex Sinpolene CPP1040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 40% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Asia Pacific) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Asia Pacific reg.. |