SABIC Innovative Plastics NORYL GTX CRN730V PPE+PA6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX CRN730V PPE+PA6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+PA+GF, FR
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 68.1 g/10 min

@Load 5.00 kg,
Temperature 280 °C
68.1 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 114 MPa
16500 psi
SABIC - Japan Method
Elongation at Break 9.0 %
9.0 %
SABIC - Japan Method
Flexural Strength 171 MPa
24800 psi
ASTM D790
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Izod Impact, Notched 1.03 J/cm
1.93 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 3.20 µm/m-°C

@Temperature -30.0 - 30.0 °C
1.78 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
32.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
17.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 197 °C

@Thickness 6.40 mm
387 °F

@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94 V-1

@Thickness 0.940 mm
V-1

@Thickness 0.0370 in
UL 94
5VA

@Thickness 2.50 mm
5VA

@Thickness 0.0984 in
UL 94
Users viewing this material also viewed the following: